A fractographic study of the effects of varying dissolved oxygen level on the cyclic crack growth of A533B steel in high temperature reactor grade water

  • Kari Törrönen
  • , Markku Kemppainen

Research output: Book/ReportReport

Original languageEnglish
Place of PublicationEspoo
PublisherVTT Technical Research Centre of Finland
Number of pages29
Publication statusPublished - 1981
MoE publication typeD4 Published development or research report or study

Publication series

SeriesVTT Metallilaboratorio. Tutkimusraportti B
Number32

Cite this