A Novel Method for cMUT fabrication
Jaakko Saarilahti
, Hannu Kattelus
, Ari Häärä
, Martti Blomberg
Research output
:
Contribution to conference
›
Conference article
›
Scientific
›
peer-review
Overview
Fingerprint
Fingerprint
Dive into the research topics of 'A Novel Method for cMUT fabrication'. Together they form a unique fingerprint.
Sort by
Weight
Alphabetically
Keyphrases
Capacitive Micromachined Ultrasonic Transducer
100%
Transducer Fabrication
100%
Silicon Nitride
75%
Fabrication Methods
50%
LPCVD Silicon Nitride
50%
Chemical Composition
25%
Deposition Rate
25%
Deposition Process
25%
Original Method
25%
Refractive Index
25%
Oxide Layer
25%
Porous Silicon
25%
Etching Rate
25%
Low Pressure Chemical Vapor Deposition (LPCVD)
25%
Mechanical Stress
25%
Top Electrode
25%
Polysilicon
25%
Deposition Parameters
25%
Process Quality
25%
Surface Micromachining Process
25%
Sealing Process
25%
HF Etching
25%
Sacrificial Oxide
25%
Transducer Characteristics
25%
Silicon Nitride Membrane
25%
INIS
fabrication
100%
ultrasonics
100%
transducers
100%
silicon nitrides
100%
chemical vapor deposition
60%
deposition
60%
layers
40%
membranes
40%
porous materials
40%
surfaces
20%
construction
20%
silicon
20%
oxides
20%
chemical composition
20%
machining
20%
electrodes
20%
refractive index
20%
etching
20%
Material Science
Silicon Nitride
100%
Transducer
100%
Low Pressure Chemical Vapor Deposition
60%
Refractive Index
20%
Micromachining
20%
Mechanical Stress
20%
Oxide Compound
20%
Porous Silicon
20%