A tool and methods for predicting pitting corrosion risk of stainless steels in evaporated conditions

    • Tero Hakkarainen Consulting
    • University of Oulu

    Research output: Chapter in Book/Report/Conference proceeding › Conference article in proceedings › Scientific › peer-review

    Original languageEnglish
    Title of host publication6th European stainless steel conference
    Subtitle of host publicationScience and market
    PublisherJernkontoret
    Pages69-74
    ISBN (Print)9789197413190
    Publication statusPublished - 2008
    MoE publication typeA4 Article in a conference publication
    Event6th European stainless steel conference: Science and market - Helsinki, Finland
    Duration: 10 Jun 2008 → 13 Jun 2008

    Conference

    Conference6th European stainless steel conference
    Country/TerritoryFinland
    CityHelsinki
    Period10/06/08 → 13/06/08