TY - CONF
T1 - Characterization of High Consistency Fiber-Foam Suspensions
AU - Prakash (PhD), Barani
AU - Laukkanen, Olli-Ville
PY - 2026/5/15
Y1 - 2026/5/15
N2 - Foam forming has recently gained significant attention in the forest-based industries for manufacturing sustainable packaging, construction, and cushioning products [1]. Traditionally, foam suspensions are prepared in mixing tanks at low wood fiber consistency (≤ 2%), which results in high water consumption. Moreover, excess moisture in the final foam-formed product must be removed through energy-intensive drying. Replacing conventional foaming methods with high-consistency wood fiber foaming offers the potential to reduce water usage, drying energy, and equipment footprint. However, increasing fiber consistency introduces complex rheological behavior [2], creating challenges in processing steps such as mixing, pumping, and uniform application on the paper machine wire. This study investigates the viscoelastic properties of high-consistency wood fiber foam suspensions. Experiments were conducted using bleached softwood kraft pulp (BSKP) and chemi-thermomechanical pulp (CTMP) with a mean fiber length of 2.0 mm and Canadian Standard Freeness (CSF) of 600 ml. Fiber consistency was varied between 8% and 12%. An 80/20 mol% mixture of sodium dodecyl sulfate (SDS) and Tween 20 (T20) served as the surfactant, with dosages ranging from 0.5 g/L to 2.0 g/L depending on fiber consistency. The laboratory foaming setup comprised a transparent acrylic tank (0.43 m tall, 0.16 m wide) equipped with a top-mounted impeller assembly (Fig-1a). For rheological characterization, a customized vane-in-cup geometry (Fig1b) was employed to minimize wall slip and confinement effects, which often limit conventional measurement geometries for fiber foams. Oscillatory tests (Fig-1c) were performed to determine viscoelastic properties. Additionally, the influence of fiber consistency (Fig-1d), air content, and carboxymethyl cellulose (CMC) addition on foam rheology was examined. Results indicate that at high fiber consistencies and air contents (~75%), wood fiber foams exhibit pronounced elasticity, with shear stiffness primarily governed by the continuous fiber network within the foam. In summary, this work provides insights into the rheological behavior of high-consistency wood fiber foam suspensions, enabling the development of sustainable packaging solutions with significantly reduced water consumption.
AB - Foam forming has recently gained significant attention in the forest-based industries for manufacturing sustainable packaging, construction, and cushioning products [1]. Traditionally, foam suspensions are prepared in mixing tanks at low wood fiber consistency (≤ 2%), which results in high water consumption. Moreover, excess moisture in the final foam-formed product must be removed through energy-intensive drying. Replacing conventional foaming methods with high-consistency wood fiber foaming offers the potential to reduce water usage, drying energy, and equipment footprint. However, increasing fiber consistency introduces complex rheological behavior [2], creating challenges in processing steps such as mixing, pumping, and uniform application on the paper machine wire. This study investigates the viscoelastic properties of high-consistency wood fiber foam suspensions. Experiments were conducted using bleached softwood kraft pulp (BSKP) and chemi-thermomechanical pulp (CTMP) with a mean fiber length of 2.0 mm and Canadian Standard Freeness (CSF) of 600 ml. Fiber consistency was varied between 8% and 12%. An 80/20 mol% mixture of sodium dodecyl sulfate (SDS) and Tween 20 (T20) served as the surfactant, with dosages ranging from 0.5 g/L to 2.0 g/L depending on fiber consistency. The laboratory foaming setup comprised a transparent acrylic tank (0.43 m tall, 0.16 m wide) equipped with a top-mounted impeller assembly (Fig-1a). For rheological characterization, a customized vane-in-cup geometry (Fig1b) was employed to minimize wall slip and confinement effects, which often limit conventional measurement geometries for fiber foams. Oscillatory tests (Fig-1c) were performed to determine viscoelastic properties. Additionally, the influence of fiber consistency (Fig-1d), air content, and carboxymethyl cellulose (CMC) addition on foam rheology was examined. Results indicate that at high fiber consistencies and air contents (~75%), wood fiber foams exhibit pronounced elasticity, with shear stiffness primarily governed by the continuous fiber network within the foam. In summary, this work provides insights into the rheological behavior of high-consistency wood fiber foam suspensions, enabling the development of sustainable packaging solutions with significantly reduced water consumption.
UR - https://wcpt10.org/assets/doc/program/Final_AbstractBook.pdf
M3 - Conference Abstract
SP - 70
EP - 71
T2 - 10th World Congress on Particle Technology, WCPT10
Y2 - 11 May 2026 through 15 May 2026
ER -