Determination of threshold potential for stress corrosion cracking of low alloy steels in high temperature, high pressure water

  • Hannu Hänninen
  • , Seija Hietanen

Research output: Chapter in Book/Report/Conference proceedingConference article in proceedingsScientific

Original languageEnglish
Title of host publicationInnovation and technology transfer for corrosion control
Subtitle of host publication11th International Corrosion Congress
Place of PublicationMilano
PublisherAssociazione Italiana di Metallurgia
Pages3.215-3.222
ISBN (Print)9788885298002
Publication statusPublished - 1990
MoE publication typeB3 Non-refereed article in conference proceedings
Event11th International Corrosion Congress - Firenze, Italy
Duration: 2 Apr 19906 Apr 1990

Conference

Conference11th International Corrosion Congress
Country/TerritoryItaly
CityFirenze
Period2/04/906/04/90

Cite this