Effect of selective dissolution on stress corrosion cracking susceptibility of austenitic and duplex stainless steels in alkaline solutions

  • Heikki Leinonen
  • , Pekka Pohjanne
  • , Tapio Saukkonen
  • , Tanja Schildt
  • , Jyrki Romu
  • , Hannu Hänninen

    Research output: Chapter in Book/Report/Conference proceedingConference article in proceedingsScientificpeer-review