Evaluation of test techniques for stress corrosion cracking of dissimilar metal weldments

  • D. Tice
  • , Aki Toivonen
  • , B. Rosborg
  • , J.D. Atkinson
  • , W. Dietzel
  • , D. Swan
  • , J. Lapena
  • , S. McAllister

    Research output: Chapter in Book/Report/Conference proceedingConference article in proceedingsScientific

    Original languageEnglish
    Title of host publicationProceedings of the 10th International Conference on Environmental Degradation of Materials in Nuclear Power Systems Water Reactors
    PublisherNational Association of Corrosion Engineers (NACE)
    Number of pages10
    Publication statusPublished - 2001
    MoE publication typeB3 Non-refereed article in conference proceedings
    Event10th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors - Lake Tahoe, United States
    Duration: 5 Aug 20019 Aug 2001
    Conference number: 10

    Conference

    Conference10th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors
    Country/TerritoryUnited States
    CityLake Tahoe
    Period5/08/019/08/01

    Cite this