Original language | English |
---|---|
Pages (from-to) | 1196-1199 |
Number of pages | 4 |
Journal | Metallurgical Transactions A: Physical Metallurgy and Materials Science |
Volume | 10 |
Issue number | 8 |
DOIs | |
Publication status | Published - 1979 |
MoE publication type | Not Eligible |
Fractographic characteristics of a hydrogen-charged AISI 316 type austenitic stainless steel
Hannu Hänninen, Tero Hakkarainen
Research output: Contribution to journal › Article › Scientific › peer-review
63
Citations
(Scopus)