High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004

Iva Betova, Martin Bojinov, Petri Kinnunen, Timo Saario, Pekka Sirkiä

Research output: Book/ReportReport

Original languageEnglish
PublisherVTT Technical Research Centre of Finland
Number of pages27
Publication statusPublished - 2004
MoE publication typeD4 Published development or research report or study

Publication series

SeriesVTT Research Report
NumberBTUO73-041298

Keywords

  • activity incorporation
  • stainless steel
  • Inconel alloy
  • decontamination
  • recontamination
  • corrosion potential (ECP)
  • redox potential
  • conductivity
  • impurities

Cite this

Betova, I., Bojinov, M., Kinnunen, P., Saario, T., & Sirkiä, P. (2004). High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004. VTT Technical Research Centre of Finland. VTT Research Report, No. BTUO73-041298
Betova, Iva ; Bojinov, Martin ; Kinnunen, Petri ; Saario, Timo ; Sirkiä, Pekka. / High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004. VTT Technical Research Centre of Finland, 2004. 27 p. (VTT Research Report; No. BTUO73-041298).
@book{6c0d3a0a7b9047969289bd4ac0fa975c,
title = "High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004",
keywords = "activity incorporation, stainless steel, Inconel alloy, decontamination, recontamination, corrosion potential (ECP), redox potential, conductivity, impurities",
author = "Iva Betova and Martin Bojinov and Petri Kinnunen and Timo Saario and Pekka Sirki{\"a}",
year = "2004",
language = "English",
series = "VTT Research Report",
publisher = "VTT Technical Research Centre of Finland",
number = "BTUO73-041298",
address = "Finland",

}

High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004. / Betova, Iva; Bojinov, Martin; Kinnunen, Petri; Saario, Timo; Sirkiä, Pekka.

VTT Technical Research Centre of Finland, 2004. 27 p. (VTT Research Report; No. BTUO73-041298).

Research output: Book/ReportReport

TY - BOOK

T1 - High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004

AU - Betova, Iva

AU - Bojinov, Martin

AU - Kinnunen, Petri

AU - Saario, Timo

AU - Sirkiä, Pekka

PY - 2004

Y1 - 2004

KW - activity incorporation

KW - stainless steel

KW - Inconel alloy

KW - decontamination

KW - recontamination

KW - corrosion potential (ECP)

KW - redox potential

KW - conductivity

KW - impurities

M3 - Report

T3 - VTT Research Report

BT - High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004

PB - VTT Technical Research Centre of Finland

ER -

Betova I, Bojinov M, Kinnunen P, Saario T, Sirkiä P. High-temperature water chemistry and activity incorporation into material samples exposed to BWR coolant at Olkiluoto 1 during the time period June 2000...May 2004. VTT Technical Research Centre of Finland, 2004. 27 p. (VTT Research Report; No. BTUO73-041298).