Impression creep testing for the HAZ of a P22 weld

  • Juhani Rantala
  • , Jan Storesund
    • Kiwa Inspecta

    Research output: Chapter in Book/Report/Conference proceeding › Conference article in proceedings › Scientific › peer-review

    Abstract

    Impression creep testing was applied in a research project funded by Värmeforsk, Sweden, in order to study the creep rate in a HAZ of a girth weld in a P22 (10CrMo910) power plant piping. In the project a special routine was developed to transfer the results of a global piping stress analysis into a detailed 3D FE model of an individual piping component. In the 3D analysis the real HAZ creep rates were modelled on the basis of the impression creep tests.
    Original languageEnglish
    Title of host publicationBaltica X
    Subtitle of host publicationInternational Conference on Life Management and Maintenance for Power Plants
    Place of PublicationEspoo
    PublisherVTT Technical Research Centre of Finland
    Number of pages7
    ISBN (Electronic)978-951-38-8436-9, 978-951-38-8435-2
    Publication statusPublished - 2016
    MoE publication typeA4 Article in a conference publication
    EventBALTICA X - International Conference on Life Management and Maintenance for Power Plants - Cruise, Helsinki-Stockholm, Finland
    Duration: 7 Jun 2016 → 9 Jun 2016

    Publication series

    SeriesVTT Technology
    Volume261
    ISSN2242-1211

    Conference

    ConferenceBALTICA X - International Conference on Life Management and Maintenance for Power Plants
    Abbreviated titleBaltica X
    Country/TerritoryFinland
    CityHelsinki-Stockholm
    Period7/06/16 → 9/06/16

    Fingerprint

    Dive into the research topics of 'Impression creep testing for the HAZ of a P22 weld'. Together they form a unique fingerprint.

    Cite this