Intermetallic dispersion-strengthened ferritic superalloys with exceptional resistance to radiation-induced hardening

  • Kan Ma*
  • , Pedro A. Ferreirós
  • , Thomas Pfeifer
  • , Robert Abernethy
  • , Sophia von Tiedemann
  • , Nianhua Peng
  • , Graeme Greaves
  • , Colin Ophus
  • , Kai Sun
  • , Anamul Mir
  • , Lumin Wang
  • , Shasha Huang
  • , Shijun Zhao
  • , Patrick Hopkins
  • , Christopher Hardie
  • , A. J. Knowles*
  • *Corresponding author for this work
  • City University of Hong Kong
  • University of Birmingham
  • University of Virginia
  • United Kingdom Atomic Energy Authority (UKAEA)
  • University of Surrey
  • University of Huddersfield
  • Stanford University
  • University of Michigan–Ann Arbor

Research output: Contribution to journalArticleScientificpeer-review

Abstract

Intermetallic dispersion-strengthening (IDS) using nano-scale coherent intermetallic precipitates offers a potent strategy to produce high-strength and radiation-resistant steels, whilst addressing the manufacturability challenges of analogous oxide dispersion-strengthened (ODS) steels. However, their performance with intermetallic stability under irradiation damage, such as radiation-induced hardening (RIH), whilst hypothesised, is undemonstrated. Here, we report on a model IDS α(A2) + α’(L21) Fe-Ni-Al-Ti ferritic superalloy, which exhibits exceptional resistance to RIH with near-zero hardening after irradiation at 300°C 1 dpa, in contrast to significant RIH in a counterpart coarse precipitate alloy (increase in nano-hardness of 1.0 GPa) and Eurofer97 (0.7 GPa). This irradiation resistance is attributed to the high density of semi-coherent precipitate-matrix interfaces, and partial-disordering L21->B2 which causes a decrease in anti-phase boundary energy. High interface density with localised interfacial strain offers effective sinks, suppressing defect populations compared to the counterpart with lower interface density. Meanwhile, atomic resolution spectroscopy and irradiation with in-situ transmission electron microscopy show that the disordering stems from Al-rich and Ti-rich sublattices mixing in the initial L21-Ni2AlTi structure below 500°C, forming metastable B2-Ni(Al,Ti). Combined, the high interface density and radiation-induced intermetallic disordering underpin the remarkable radiation tolerance, demonstrating the IDS concept as a promising radiation-resistant materials design strategy.
Original languageEnglish
Article number121095
JournalActa Materialia
Volume293
DOIs
Publication statusPublished - 1 Jul 2025
MoE publication typeA1 Journal article-refereed

Funding

A.J. Knowles gratefully acknowledges funding from EPSRC EP/T016566/1, UKRI Future Leaders Fellowship MR/T019174/1 & MR/Y034155/1, and Royal Academy of Engineering Research Fellowship RF\201819\18\158. A. J. Knowles, C. Hardie and S. von Tiedemann gratefully acknowledge the funding from the NEUtron iRradiatiOn of advaNced stEels (NEURONE) programme via Fusion Futures. A. J. Knowles and K. Ma thank the European Union's Horizon 2020 research and innovation programme under grant agreement No 958418 “COMPASsCO2” (https://www.compassco2.eu). The work at the University of Virginia was supported from the Office of Naval Research, Grant Number N00014-21-1-2477. The atom probe facility at the University of Oxford is funded by EPSRC grant EP/T011505/1, and access was supported by UKRI-NNUF EP/T011351/1 (Call 7 Application 88). K. Ma and A. J. Knowles thank Dr Christina Hofer and Dr Paul Bagot for their support in APT data collection, data analysis and fruitful discussion. The authors also acknowledge the Diamond Light Source UK for time on beamline I11 under proposal CY32708, supported by Dr Sarah Day. Work at the Molecular Foundry was supported by the Office of Science, Office of Basic Energy Sciences, of the U.S. Department of Energy under Contract No. DE-AC02-05CH11231. K. Ma acknowledges the support of Dr Karen Bustillo and Dr Stephanie Ribet on the 4D-STEM experiment. K. Ma and P. A. Ferreirós acknowledge EPSRC grants EP/M028283/1 for funding the MIAMI-2 system construction and EP/X015491/1 for the UKNIBC access scheme.

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure

Keywords

  • Dislocation
  • Disordering
  • Interface
  • Intermetallic dispersion-strengthening
  • Radiation-induced hardening

Fingerprint

Dive into the research topics of 'Intermetallic dispersion-strengthened ferritic superalloys with exceptional resistance to radiation-induced hardening'. Together they form a unique fingerprint.