Long term creep tests on timber beams in heated and non-heated environments

Shankare Gowda, Markku Kortesmaa, Alpo Ranta-Maunus

Research output: Book/ReportReport

2 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Long term creep tests on timber beams in heated and non-heated environments'. Together they form a unique fingerprint.