Low-temperature atomic layer deposition of SiO2/Al2O3 multilayer structures constructed on self-standing films of cellulose nanofibrils

Matti Putkonen, Perttu Sippola, Laura Svärd, Timo Sajavaara, Jari Vartiainen, Iain Buchanan, Ulla Forsström, Pekka Simell, Tekla Tammelin (Corresponding Author)

Research output: Contribution to journalArticleScientificpeer-review

4 Citations (Scopus)