| Original language | English |
|---|---|
| Title of host publication | Proceedings of the 6th International Congress on Metallic Corrosion |
| Subtitle of host publication | Extended Abstracts |
| Editors | F. Burns, J. Moresby, P. Thorpe |
| Place of Publication | Sydney |
| Publisher | Australasian Corrosion Association |
| Pages | 422-429 |
| ISBN (Print) | 978-0-9597454-0-5 |
| Publication status | Published - 1975 |
| MoE publication type | A4 Article in a conference publication |