Selective dissolution and stress corrosion cracking susceptibility of austenitic and duplex stainless steels in sodium sulfide containing alkaline solutions

  • Heikki Leinonen
  • , Pekka Pohjanne
  • , J. Romu
  • , T. Saukkonen
  • , T. Schildt
  • , H. Hänninen
    • Aalto University

    Research output: Chapter in Book/Report/Conference proceedingConference article in proceedingsScientificpeer-review

    Fingerprint

    Dive into the research topics of 'Selective dissolution and stress corrosion cracking susceptibility of austenitic and duplex stainless steels in sodium sulfide containing alkaline solutions'. Together they form a unique fingerprint.