Stress corrosion cracking initiation susceptibility of Alloy 182 with different surface treatments

Zaiqing Que (Corresponding Author), Timo Saario, Aki Toivonen, Ulla Ehrnstén

    Research output: Contribution to journalArticleScientificpeer-review