Stress corrosion cracking susceptibility of TIG welded and HIP bonded 316L(N) stainless steel

Seppo Tähtinen, Anna-Maija Kosonen, Laura Taivalaho

Research output: Book/ReportReport

Original languageEnglish
PublisherVTT Technical Research Centre of Finland
Number of pages29
Publication statusPublished - 2002
MoE publication typeD4 Published development or research report or study

Publication series

SeriesVTT Research Report
NumberBTUO73-021064

Keywords

  • stress corrosion cracking
  • stainless steel
  • slow strain rate test
  • TIG weld
  • HIP joint