Stress corrosion cracking tests for low and high alloy steels in sour oilfield service: Tests performed at VTT

Kari Saarinen, Esa Hämäläinen

Research output: Book/ReportReport

Fingerprint

Dive into the research topics of 'Stress corrosion cracking tests for low and high alloy steels in sour oilfield service: Tests performed at VTT'. Together they form a unique fingerprint.

Engineering & Materials Science