Sulphide induced stress corrosion cracking of copper: Final Report

  • Esko Arilahti
  • , Leena Carpen
  • , Taru Lehtikuusi
  • , Markus Olin
  • , Timo Saario
  • , Päivi Varis

    Research output: Book/Report › Report

    Original languageEnglish
    Place of PublicationEspoo
    PublisherVTT Technical Research Centre of Finland
    Number of pages14
    Publication statusPublished - 2011
    MoE publication typeD4 Published development or research report or study

    Publication series

    SeriesVTT Research Report
    NumberVTT-R-00467-11