Skip to main navigation Skip to search Skip to main content

Surface analysis of tiles and samples exposed to the first JET campaigns with the ITER-Like Wall

  • J.P. Coad
  • , E. Alves
  • , C.F. Ayres
  • , N. Baradas
  • , A. Baron-Wiechec
  • , K. Heinola
  • , Jari Likonen
  • , G.F. Matthews
  • , A. Widdowson
  • , JET-EFDA contributors

    Research output: Chapter in Book/Report/Conference proceedingConference abstract in proceedingsScientific

    Original languageEnglish
    Title of host publication14th International conference on plasma-facing materials and components for fusion applications, Jülich, 2013
    Subtitle of host publicationBook of abstracts
    Place of PublicationJülich
    Pages46
    Publication statusPublished - 2013
    MoE publication typeNot Eligible
    Event14th International conference on plasma-facing materials and components for fusion applications: PFMC-14 - Jülich, Germany
    Duration: 13 May 201317 May 2013

    Conference

    Conference14th International conference on plasma-facing materials and components for fusion applications
    Abbreviated titlePFMC-14
    Country/TerritoryGermany
    CityJülich
    Period13/05/1317/05/13

    UN SDGs

    This output contributes to the following UN Sustainable Development Goals (SDGs)

    1. SDG 7 - Affordable and Clean Energy
      SDG 7 Affordable and Clean Energy

    Cite this