The biaxial creep testing device, Crebello

Research output: Book/ReportReport

Original languageEnglish
Place of PublicationEspoo
PublisherVTT Technical Research Centre of Finland
Number of pages23
Publication statusPublished - 2014
MoE publication typeD4 Published development or research report or study

Publication series

SeriesVTT Research Report
NumberVTT-R-01863-14

Keywords

  • material
  • high temperature
  • pneumatic
  • testing
  • biaxial creep

Cite this

Moilanen, P., & Ehrnstén, U. (2014). The biaxial creep testing device, Crebello. VTT Technical Research Centre of Finland. VTT Research Report, No. VTT-R-01863-14