Abstract
Atomic layer deposition (ALD) is a chemical vapour deposition (CVD)
technique that is especially suited for manufacturing conformal inorganic
material layers on complex 3D substrates. Unlike other CVD processes, ALD
relies on the systematic use of self-terminating gas-solid reactions, enabling
a highly reproducible growth of extremely uniform inorganic layers with
thicknesses down to fractions of nanometres. ALD has a four-decade history,
and in some technological aspects, ALD can be considered a mature technique.
In other aspects, however, ALD is still at a developing, rapidly progressing
stage. For example, the selection of metal reactants suitable for ALD
processing is expanding due to world-wide research efforts. The main purpose
of this work is to review the current knowledge of the surface chemistry of
ALD processes, with the well-known near-ideal trimethylaluminium/water process
to deposit aluminium oxide and occasionally other processes as examples. Open
questions regarding the understanding of the surface chemistry of ALD,
waiting for their answers, will be pointed out.
| Original language | English |
|---|---|
| Title of host publication | 16th European Conference on Chemical Vapor Deposition, EuroCVD-16 |
| Subtitle of host publication | Book of Extended Abstracts |
| Editors | Chris R. Klein |
| Publisher | Delft Technical University |
| Publication status | Published - 2007 |
| MoE publication type | Not Eligible |
| Event | 16th European Conference on Chemical Vapor Deposition, EuroCVD-16 - The Hague, Netherlands Duration: 16 Sept 2007 → 21 Sept 2007 |
Conference
| Conference | 16th European Conference on Chemical Vapor Deposition, EuroCVD-16 |
|---|---|
| Country/Territory | Netherlands |
| City | The Hague |
| Period | 16/09/07 → 21/09/07 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 9 Industry, Innovation, and Infrastructure
Keywords
- Atomic layer deposition
- ALD
- Al2O3
- trimethylaluminum
- trimethylaluminium
- surface chemistry
Fingerprint
Dive into the research topics of 'Understanding the surface chemistry of atomic layer deposition: Achievements and challenges'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver