X-ray reflectivity characterization of atomic layer deposition Al 2O3/TiO2 nanolaminates with ultrathin bilayers

Sakari Sintonen, Saima Ali, Oili M.E. Ylivaara, Riikka L. Puurunen, Harri Lipsanen

    Research output: Contribution to journalArticleScientificpeer-review

    19 Citations (Scopus)

    Fingerprint Dive into the research topics of 'X-ray reflectivity characterization of atomic layer deposition Al <sub>2</sub>O<sub>3</sub>/TiO<sub>2</sub> nanolaminates with ultrathin bilayers'. Together they form a unique fingerprint.

    Chemical Compounds

    Engineering & Materials Science

    Physics & Astronomy